Composition of vetonit finishing putty. Vetonit putty vh technical characteristics

Designed for leveling walls and ceilings in dry and wet areas

Before applying cement plaster mixture Vetonit TT Vetonit

It is necessary to prepare the surface. The base is cleaned of dust, dirt, greasy stains, loose old peeling building materials. The surface should be hard, dry, without large irregularities.

Preparation of mortar (mixing).
Kneading construction mixture produced in a clean container. Water for congestion cement mixture should be at room temperature. Dry mix Vetonit falls asleep in water. Mixing mechanically using a mixer for at least 1 minute.
MIXING
Dry plasterVetonit mixed with clean water room temperature in a mixer. Mixing time (if a whole bag is mixed) is 1 minute. For mixing Vetonit TT plaster mixture Weber Vetonit 6 liters of water are used. Received building mixture should be homogeneous without lumps and let it sit for 15 minutes. After this, the building cement must be mixed again for 30 seconds and the solution is ready for use. Working temperature Vetonit TT solution should not fall below +10 C. Open time ready construction mixture Vetonit is 4 hours at a temperature of +20 C. During this time, the Vetonit TT solution must be consumed.
Work order

Very dry and highly absorbent substrates must be treated with a primer. When applied locally plaster Vetonit Vetonit the thickness should not be more than 30 mm in one pass.
When completely applying the plaster mixture Vetonit TT uses a ruler to draw a solution 60 - 80 cm long. Construction worksya on cement based applied with a spatula to the prepared surface from bottom to top, after which the mortar is pulled out using a rule. Excess mortar is cut off with a spatula and used in further work. Thickness cement solution in one pass should be from 1 to 10 mm. To apply a second coat, it is necessary to allow the first layer to dry for 1 to 2 days. dried out layer of plasters and is sanded and before applying the next layer of mortar in dry rooms, the surface is moistened or primed.

After the end of the plastering works all tools must be cleaned of undried Vetonit mortar Vetonit and rinse. The water that was used to wash the tools cannot be used in the future for mixing the plaster solution.


Walls and ceilings that were prepared using construction mixture Vetonit TT can be used for tiling with ceramic tiles, as well as for further final leveling. In wet and wet rooms high humidity it is necessary to use Vetonit V+VH putty. In damp rooms and with increased mechanical load, putties are most suitable Vetonit B+BX. In dry rooms, Vetonit L+LR or Vetonit T+KR are used for puttying.

Technical characteristics of the plaster mixture
Mix color - gray
Water resistance of plaster: waterproof
Binders Vetonit TT: cement
Viability of mortar: 4 hours after mixing with water
Drying time: depending on the thickness of the plaster layer and temperature 1 day Consumption: approx. 1.2 kg/sq.m/1mm.
Layer application thickness: with partial leveling of walls and ceilings maximum 30mm, with full leveling maximum 2-10mm/1 layer
Fraction: maximum 1.0mm.
The operating temperature of the Vetonit TT solution should not fall below +10 C Additional Tips In the Vetonit product line, Vetonit Dispersion liquid is a special solution that increases the strength characteristics of plaster. This solution must be added to the water that will be used when mixing with the cement mortar Vetonit TT from a ratio of 1 to 10. Excess mortar or residues of the Vetonit TT dry mixture must be disposed of and in no case should the mortar be washed through the sewer, because this can lead to its failure (clogging) Plaster mixture not suitable for application on surfaces coated with paint, leveled with lime leveler, water-soluble substances, Vetonit T, Vetonit KR, L, LR. Cement plaster not suitable for leveling floors.
Packaging and safety precautions Dry cement mortar Weber Vetonit Packed in 25 kg paper bags and stored in dry rooms in original packaging.

Avoid prolonged contact of the Vetonit TT plaster mixture with open areas skin, contact of the mixture with the mucous membrane of the eyes, Airways. If the solution gets into your eyes, rinse them with running water.

Vetonit putty, which is based on white cement and limestone, is used for the final leveling of walls and ceilings made of concrete, expanded clay concrete, brick, and plastered surfaces. It is used for interior and exterior work and facade finishing. The treated surface with this mixture can subsequently be covered with wallpaper or painted with various water-based, latex, acrylic paints or glue ceramic tiles. This mixture meets all GOST requirements. You can buy it from our company.

Specifications:

Blend color

White gray

White cement

Water resistance

waterproof

Aggregate

limestone

Maximum filler fraction, mm

Consumption of dry mixture kg/m2

Consumption clean water, 10 kg/l

From 3.2 to 3.6

Clean water consumption, l/25 kg bag

Thickness of application of one layer

Time of use from the moment it is mixed with water

Strength of adhesion of mortar to concrete after 28 days

Drying time of one layer of solution at 20°C

Compressive strength after 28 days, relative humidity 50%, +23°С

Set 50% mortar strength

Material packaging

Bag 25 and 5 kg

The basis

Must be clean, hard and dust-free. Substances that weaken adhesion such as oil, dust, etc. must be removed from the surface. Items that will not be processed must be carefully protected. If necessary, very dry surfaces are moistened.

Kneading

A 25 kg bag of dry mixture is mixed with 8-9 liters of clean water (32-36% of the weight of the dry mixture). Mixing is done using a powerful drill with an attachment for 1-2 minutes. For the best dissolution of the binder, the putty mixture is allowed to sit for 15 minutes. After re-mixing, the mixture is ready for use. The mortar mixture is suitable for use within 3 hours from the moment of mixing with water (at +20 o C). The temperature of the mortar mixture should be above +10 o C.

Completing of the work

The mortar mixture is applied mechanically by spraying or manually using a two-handed spatula. For partial leveling, use a small steel spatula 30 cm wide. The excess mixture is removed and used again. If leveling is carried out in several layers, you need to make sure that the previous layer is completely dry (within 1-2 days).
The dry surface is sanded with thin sanding paper after each coat and dust is removed before painting.

Cleaning the instrument

Working tools and equipment used are washed with water immediately after completion of work.

Add. operations

In dry conditions, in order to provide the necessary conditions for hardening, the leveled surface is moistened with water using a sprayer.

INSTRUCTIONS FOR USE

Preparing the base

The base must be clean, hard and durable. Windows and other untreated surfaces must be carefully protected. Substances that weaken adhesion such as grease, dust, etc. must be removed. The temperature of the base and mortar mixture must be at least +10 ° C.

Preparing the mixture

Gradually pour a bag (20 kg) of dry mixture into a container with 7.2 - 7.6 liters of water, stirring at the same time. Recommended water temperature + 20°C. Mixing is carried out using a drill with an attachment for 3-5 minutes. Let the solution sit for 10 minutes. After this, stir the mixture again before use. Usage time ready mixture 1.5 hours from the moment of mixing with water.

Application

The mortar mixture is applied by mechanical spraying or manually and leveled using a steel spatula. For complete leveling, use a two-handed steel spatula 80 cm wide, and for partial leveling, use a small one, 30 cm wide. When leveling in several layers, it is necessary to apply each subsequent layer on the completely dry previous one (after 1-2 days). The dried surface of the putty must be treated with sanding paper and removed from dust before applying the next layer. When leveling the surfaces of facades, it is recommended to apply the mortar mixture in 2 layers. The first layer is partial leveling and filling of pores. The second layer is to completely level the surface.

In dry conditions to ensure necessary conditions After hardening, the leveled surface is moistened with water using a sprayer. After processing sandpaper The leveled and dried surface can be painted with alkali-resistant (cement-resistant) paint, covered with wallpaper or tiled, having previously removed dust from the surface after sanding. To increase the wear resistance of the material and improve adhesion, you can replace 10% of the mixing water weber.vetonit MD16. When leveling old painted surfaces, tile adhesive can be used as an adhesion layer. weber.vetonit ultra.fix or base layer perform with solution weber.therm S100. Facade surfaces can be painted facade paints weber.ton akrylat And weber.ton micro V.

The drying time of one layer of recommended thickness is 1-2 days with good ventilation. Drying time depends on layer thickness, ventilation and temperature. A level of 50% of the final strength is achieved within 7 days at 20°C; as the temperature decreases, the process of strength gain slows down.

CLEANING THE INSTRUMENT

Working tools and equipment are washed with water immediately after completion of work.

PRECAUTIONARY MEASURES

When working, you must use rubber gloves; avoid contact with skin and eyes; In case of contact with eyes, rinse big amount water; keep away from children.

DISPOSAL INSTRUCTIONS

The dry mixture and hardened material must be disposed of as construction waste. The material must not be discharged into the sewer. Dispose of the paper bag as regular waste.

And bases treated with Vetonit TT, TT Light, Perlite putty or plaster solutions Serpo 410 Tinrender and Serpo 414 Unirender. If necessary, the leveled surface can be additionally painted; when painting facade surfaces, use only silicate paint. Attention! The mixture is not suitable for application on surfaces leveled with water-soluble leveling mixtures, such as Vetonit L, T, LR+ and KR putty; for application on surfaces plastered with weak lime plasters. The mixture is also not suitable for leveling floors.

Technical data of Vetonit VH putty white

White color

Water resistance: waterproof

Binder: cement

Filler: limestone,

Operating temperature: during execution, the temperature of the base, mortar mixture and room must be above +10°C

Time of use: approximately within 3 hours from the moment of mixing with water

Compressive strength: 6-8 MPa after 28 days at a relative humidity of 65% and a temperature of +23°C

Hardening: reaches approximately 50% of the final strength within 7 days; in cold weather the process of gaining strength slows down

Consumption: approximately 1.2 kg/m2 with a layer thickness of 1 mm

Required amount of water: 8-9 liters per 25 kg of dry mixture

Adhesion strength to concrete: > 0.5 MPa after 28 days at a relative humidity of 65% and a temperature of +23°C

Preparing the base for working with Vetonit VH putty white

The base must be clean, hard and dust-free. Substances that weaken adhesion such as grease, dust, etc. must be removed. Windows and other untreated surfaces must be carefully protected. If necessary, dry and absorbent surfaces are moistened.

Mixing with Vetonit VH white putty

A bag of dry mixture (25 kg) is mixed with 8-9 liters of clean water. Mixing is done with a powerful drill with an attachment for 3-5 minutes. To better dissolve the binder, the mixture is allowed to stand for about 10 minutes. After light re-stirring, the mortar mixture is ready for use. The mortar mixture is suitable for use within approximately 3 hours from the moment of mixing with water. The temperature of the mortar mixture must be above +10°C. Working tools and equipment are washed with water immediately after use. Attention! Do not pour the mortar mixture down the drain to avoid clogging the pipes.

Carrying out work with Vetonit VH putty white

The mortar mixture is applied mechanically by spraying or manually using a steel spatula. For complete leveling, use a two-handed steel spatula 80 cm wide; for partial leveling, a smaller steel spatula 30 cm wide is used. Excess mortar mixture is removed and used again. If leveling is carried out in several layers, each time you need to make sure that the previous layer is completely dry (within 1-2 days). The dried surface is sanded with thin sandpaper after each layer. When leveling the surfaces of facades, it is recommended to apply the mortar mixture in 2 layers. The first layer is partial leveling and filling of pores. The second layer is to completely level the surface. The leveled surface is rubbed down, for example, with thin sanding paper and the sanding dust is removed by starting painting work. In dry conditions, to ensure the necessary conditions for the hardening process, the leveled surface is moistened with water using a sprayer.

Final surface treatment and additional recommendations for working with Vetonit VH white putty

The leveled, hardened surface can be painted with alkali-resistant (cement-resistant) paint, covered with wallpaper or tiled. If necessary, a contaminated leveled surface can be cleaned with water, any usual cleaning agents, or re-coated with Vetonit LR+, LR Fine, KR or KR Fine putty indoors, and with Vetonit VH putty outside buildings. Tiling can be done by using suitable Vetonit and laying the tiles directly onto the Vetonit VH hardened surface, following the tiling instructions. The surfaces of the facades can be painted with lime-cement paint Serpo 244, silicate paint Serpo 303, silicone paint Serpo or various high-quality silicone emulsion paints.

Useful tips for working with Vetonit VH putty white

To increase the wear resistance of the material and improve adhesion, you can replace 10% of the mixing water with Vetonit Dispersion (approximately 1 liter of Dispersion per 25 kg of dry mixture). When leveling old painted surfaces, Vetonit glue can be used as an adhesive layer for repair work or the base layer can be done with Serpo 410 Thinrender solution.

Shelf life in closed packages in dry rooms is 12 months from the date of manufacture.

Weber.vetonit vh - weber vetonit

Preparing the base

The base must be solid, clean, free from dust and dirt. Substances that weaken adhesion such as grease, dust, etc. must be removed. If necessary, dry and absorbent surfaces are moistened. Windows and other untreated surfaces must be carefully protected.

Preparing the mixture

Pour 8-9 liters of clean water into a container and add 25 kg (bag) of the mixture weber.vetonit VH, and the mixture must be added to water, and not vice versa. Recommended water temperature is 20°C. Mixing is done with a powerful drill with an attachment for 3-5 minutes. To better dissolve the binder, the mixture is allowed to stand for 10 minutes. After light re-stirring, the mixture is ready for use. The mortar mixture is suitable for use within 3 hours from the moment of mixing with water. The temperature of the mortar mixture should be in the range from +10 to 30° C.

Application

The mortar mixture is applied by mechanical spraying or manually and leveled using a steel spatula. For complete leveling, use a two-handed steel spatula 80 cm wide, and for partial leveling, use a small one, 30 cm wide. When leveling in several layers, it is necessary to apply each subsequent layer on the completely dry previous one (after 1-2 days). The dried surface of the putty must be treated with sanding paper and removed from dust before applying the next layer. When leveling the surfaces of facades, it is recommended to apply the mortar mixture in 2 layers. The first layer is partial leveling and filling of pores. The second layer is to completely level the surface.

In dry conditions, to ensure the necessary hardening conditions, the leveled surface is moistened with water using a sprayer. After sanding, the leveled and dried surface can be painted with alkali-resistant (cement-resistant) paint, wallpapered or tiled, having previously removed dust from the surface after sanding. To increase the wear resistance of the material and improve adhesion, you can replace 10% of the mixing water weber.vetonit MD16. When leveling old painted surfaces, glue can be used as an adhesive layer. weber.vetonit RF or make the base layer with a solution weber.vetonit 410. Facade surfaces can be painted with facade paints weber.vetonit420 And weber.ton micro V.

Drying time

The drying time of one layer of recommended thickness is 1-2 days with good ventilation. Drying time depends on layer thickness, ventilation and temperature. A level of 50% of the final strength is achieved within 7 days at 20°C; as the temperature decreases, the process of strength gain slows down.

Vetonit vh - from construction discount! Wholesale and Retail. delivery in St. Petersburg

Finishing putty Vetonit VH

Vetonit VH finishing putty based on white cement and limestone is used for finishing leveling the surface of walls and ceilings made of concrete, lightweight concrete, expanded clay concrete, brick, plastered surfaces, including the surfaces of Vetonit TT, TTT, 410, 414 plasters. Vetonit putty can used for exterior work on facades. The surface treated with Vetonit VH putty can subsequently be covered with wallpaper or painted with various water-based, latex or acrylic paints, or ceramic tiles can be glued onto it. When working with Vetonit VH putty, it is possible to apply it to the surface of walls and ceilings using such mixing and injection machines as "Monojet PFT" (G4), (G5). This Vetonit VH putty meets all GOST requirements.

Features and composition of Vetonit VH putty:

  • Possibility of using Vetonit VH putty for interior and exterior work for finishing rooms with high humidity and finishing the façade of a building.
  • When applying Vetonit putty by machine, high productivity is ensured, which is approximately 2 - 3 times more than in comparison with manual application of Vetonit putty on the leveled surface.
  • When using Vetonit putty, a smooth and durable surface is provided on which, in the future, it is possible to stick ceramic tiles, or paint with various water-based, latex or acrylic paints.
  • The maximum layer of Vetonit VH finishing putty is from 1 to 2 mm.
  • Low putty Vetonit, amounting to only 1.2 kg per 1 m2 of treated surface, allows you to save your material resources.
  • The Vetonit finishing putty is made from environmentally friendly white cement and a lime component with a maximum filler fraction of up to 0.3 mm and gives the Vetonit solution increased adhesive properties to the solution. The composition of this Vetonit dry mixture does not contain any substances harmful to human health and complies with all current hygienic standards and GOST standards in the Russian Federation.

Vetonit VH putty consumption:

The consumption rate of Vetonit putty with a layer thickness of 1 mm/m² is about 1.2 kg per 1 m2. Depending on the professional skills of the workers performing finishing work and without taking into account material losses.

Preparatory work and conditions for working with Vetonit VH putty:

Before you start finishing works with Vetonit putty, the surface to be treated must be thoroughly cleaned of bitumen, dirt, oil, dust, lime, grease, residues of mineral and organic paints and adhesives, as well as various water-soluble substances that interfere with the adhesion of Vetonit putty to the treated surfaces, as well as the structural support . If the surface is too dry, before applying Vetonit putty, it must be pre-treated with Vetonit MD-16 primer. Vetonit must be applied by roller, brush, spray or brush. The coating used for surface treatment must form the required thin continuous layer of up to 1 mm, but without allowing the formation of drips on horizontal surfaces. Surfaces that have increased water absorption must be treated with a primer twice. The required quality of surfaces treated with primer should be determined by the absence of water absorption into the treated surface. Re-contamination of primed surfaces is not permitted. Surfaces treated with a primer have reduced water absorption and increased adhesive properties. When working with Vetonit putty and for the next 3 days, you must adhere to temperature regime within the range from +10°С to +20°С. The base of the surface will be ready for application of the Vetonit finishing putty only after the primer mixture has completely dried.

Preparation of Vetonit VH putty:

To work with Vetonit putty solution, it must be prepared with the following proportions: using mixing and pumping devices with a constantly dosed water supply, the proportion is selected experimentally. These proportions must be remembered so that subsequent batches of Vetonit putty solution are prepared with the same consistency. Immediately before starting work on applying the Vetonit putty solution to the surface to be treated and during the work, you need to constantly check the spreadability of the prepared Vetonit putty solution. manual application Vetonit putty solution is prepared according to the following proportions: when mixing 10 kg of dry Vetonit mixture, you will need approximately 3.2 to 3.6 liters of water from the drinking water supply at a temperature of 20°C. To mix one 25 kilogram bag of Vetonit dry construction mixture, you will need about 8 to 9 liters of clean water from the drinking water supply. Vetonit dry putty mixture is poured into a pre-prepared amount drinking water from room temperature and mixed for about 3-5 minutes using an electric drill with an attachment or an electric mixer, with a maximum rotation speed of these tools not exceeding 600 rpm. . To obtain a homogeneous consistency from the prepared Vetonit putty solution, then let the Vetonit putty solution sit for about 5 minutes and then mix it again, after which the Vetonit putty solution will be ready for use. Maximum working time with prepared cement mortar mixture putty mixture Vetonit is about 3 hours at a temperature of 20°C. After completing the work in the next 3 days, you need to prevent direct contact with the finished surface. sun rays, drafts and frosts.

The procedure for working with the Vetonit VH finishing putty mortar mixture:

Vetonit putty can be applied either manually or mechanically. For continuous finishing of flat plastered surfaces, the initial layer of Vetonit putty solution is applied and leveled using a wide 800 mm trowel. When partially finishing the surface, leveling can be done with a smaller spatula up to 300 mm. After that, the dried and hardened surface must be cleaned with special abrasive materials and only after this is it possible to apply an additional layer of Vetonit putty solution. After the Vetonit putty has completely dried for 1 to 2 days, you can clean the treated surface using a grinding tool (a grater with sandpaper or a sanding mesh). Before carrying out subsequent work and to increase the strength of the finished base, the surface must be primed with Vetonit MD-16 primer.

Recommendations and precautions when using Vetonit VH cement putty:

When preparing a mortar mixture of Vetonit putty, an overdose of water is unacceptable, which can lead to a deterioration in the physical and strength properties of the mortar mixture of Vetonit putty. And to increased shrinkage of the mortar mixture of Vetonit VH putty and can subsequently lead to cracking of the finished treated surface. When working with Vetonit VH putty, it is necessary to regularly mix the prepared Vetonit putty mortar mixture and do not allow additional dilution of the Vetonit VH putty mortar mixture with water. When the Vetonit VH putty solution sets after the expiration of its use, additional introduction of water will not help, since the solution loses its adhesive qualities. When working with Vetonit VH putty, you must adhere to the instructions for carrying out general construction work, as well as safety precautions at construction sites.

When working with Vetonit VH putty, you must use construction gloves, and also avoid getting Vetonit VH putty in your eyes and skin. If Vetonit VH putty gets into your eyes, rinse immediately with plenty of water and consult a doctor. Keep away from children!

Technical characteristics for Vetonit VH putty:

Material color

White gray

Binder

White cement

Water resistance of the material

waterproof

Filler material

limestone

Maximum filler fraction, mm

Consumption of dry mixture kg/m2/mm

Clean water consumption, 10 kg/l

From 3.2 to 3.6

Clean water consumption, l/25 kg bag

Time of application of the solution from the moment it is mixed with water, hours

The adhesion strength of the mortar to concrete after 28 days, MPa, is at least

Drying time of one layer of solution at 20°C, days

The compressive strength of the mortar after 28 days, relative humidity 50%, +23°C, MPa is not less than

Gain 50% solution strength within 24 hours

Material packaging

Paper bag 25 and 5 kg

Manufacturer's warranty and storage and transportation conditions for Vetonit VH putty:

The manufacturer guarantees that Vetonit VH putty meets all the requirements of 31357-2007, subject to the consumer's compliance with all storage, transportation conditions and the instructions provided.

Does not bear any responsibility if the consumer fails to comply with the technology for working with this material, as well as if it is used for purposes and conditions that are not provided for in these instructions.

The deviation from net weight corresponds to GOST R 8.579-2001.

Vetonit products are approved for use in all types civil engineering(Aeff

Bags of Vetonit VH dry mix must be stored in covered, dry rooms that ensure the preservation of the packaging and protect them from moisture. The shelf life of the dry mixture in the manufacturer's container is 12 months from the date of manufacture.

We offer you Vetonit VH for low prices wholesale and retail in our online store in St. Petersburg.

We provide delivery services in St. Petersburg and Leningrad region, we carry out lifting materials to the floor.

 
Articles By topic:
Purulent adnexitis symptoms and treatment
(salpingoophoritis) is an inflammatory process with simultaneous involvement of the ovaries and fallopian tubes (uterine appendages). In the acute period, it is characterized by pain in the lower abdomen, more intense from inflammation, elevated temperature, and signs of intoxication. Mo
Benefits on a social card for a pensioner in the Moscow region
In the Moscow region, various benefits are provided for pensioners, since they are considered the most socially vulnerable part of the population. Benefit – full or partial exemption from the conditions for fulfilling certain duties, extending to
What will happen to the dollar in February
What will the dollar exchange rate be at the beginning of 2019? How will the cost of a barrel affect the dynamics of the dollar/ruble pair? What will prevent the ruble from strengthening against the USD at the beginning of 2019? You will learn about all this in the dollar exchange rate forecast for the beginning of 2019.
Analytics economic
Hello, dear inquisitive practitioners. Why did he greet you in this way? Well, of course! After all, unlike other readers, you immediately transform all the knowledge gained into tangible, tasty objects that disappear just as quickly as